The focus of this study was the investigation of the quasi-simultaneous laser welding (QSW) technique of polymethyl methacrylate (PMMA) and acrylonitrile butadiene styrene (ABS) in a T-joint configuration using a circular wobble laser path. The main aim was to find how laser parameters, such as scanning speed, number of scans, and laser power, influence key indicators of weld quality: penetration depth and weld strength. A range of scanning speeds (1–2 m/s) and scan repetitions (20–70) was explored, with the goal of keeping the total welding time around 1 s, a time compatible with industrial mass production. The results demonstrated a clear correlation between linear energy density and penetration depth. Deeper penetrations were achieved at higher energy levels. Weld strength was maximized with a lower number of scans (20) and higher powers (above 130 W). The configuration offering the best combination of weld strength (1137 N) and total welding time (0.8 s) was identified, demonstrating the suitability of QSW for mass production

Analysis of Quasi-Simultaneous Laser Welding in T-Joint Configuration for PMMA-ABS Using Circular Wobble Geometry / Lezzoche, Antonio; Mossotti, Giulia; Nicosia, Carmelo; Baggi, Marco; Perlo, Michele; Scaltrito, Luciano; Ancillao, Andrea. - In: MATERIALS. - ISSN 1996-1944. - 18:21(2025). [10.3390/ma18214819]

Analysis of Quasi-Simultaneous Laser Welding in T-Joint Configuration for PMMA-ABS Using Circular Wobble Geometry

Lezzoche, Antonio;Mossotti, Giulia;Nicosia, Carmelo;Scaltrito, Luciano;Ancillao, Andrea
2025

Abstract

The focus of this study was the investigation of the quasi-simultaneous laser welding (QSW) technique of polymethyl methacrylate (PMMA) and acrylonitrile butadiene styrene (ABS) in a T-joint configuration using a circular wobble laser path. The main aim was to find how laser parameters, such as scanning speed, number of scans, and laser power, influence key indicators of weld quality: penetration depth and weld strength. A range of scanning speeds (1–2 m/s) and scan repetitions (20–70) was explored, with the goal of keeping the total welding time around 1 s, a time compatible with industrial mass production. The results demonstrated a clear correlation between linear energy density and penetration depth. Deeper penetrations were achieved at higher energy levels. Weld strength was maximized with a lower number of scans (20) and higher powers (above 130 W). The configuration offering the best combination of weld strength (1137 N) and total welding time (0.8 s) was identified, demonstrating the suitability of QSW for mass production
2025
File in questo prodotto:
File Dimensione Formato  
MDPI_materials_AL.pdf

accesso aperto

Tipologia: 2a Post-print versione editoriale / Version of Record
Licenza: Creative commons
Dimensione 2.72 MB
Formato Adobe PDF
2.72 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/3004403