Digital light processing (DLP) enables the fabrication of geometrically complex alumina components, but printing-induced defects and build-orientation effects still limit their mechanical reliability, particularly at elevated temperature. This study investigates how exposure parameters and build orientation influence defect evolution, surface topography, elastic stiffness, and flexural strength of DLP-printed alumina. Rectangular bars were manufactured in vertical and horizontal orientations using a standard exposure strategy and the modified condition with a constant exposure energy of 350 mJ cm−2. X-ray computed tomography (XCT) was used to track dimensional changes and XCT-resolved defects after pre-conditioning, debinding, and sintering. Surface topography was evaluated by profilometry, dynamic Young's modulus was measured with Impulse Excitation Technique (IET) from room temperature to 1200 °C, and four-point flexural tests were performed at room temperature and 1100 °C. Exposure modification reduced the sintered XCT-resolved porosity from 0.10 to 0.01% in the vertical orientation and from 0.23 to 0.06% in the horizontal orientation. The median equivalent defect diameter decreased from 85 to 51 μm and from 69 to 42 μm, respectively. Modified specimens exhibited higher dynamic Young's modulus during heating, while all configurations retained approximately 86-88% of their room-temperature stiffness at 1100 °C. Within the limited flexural dataset, based on one or two specimens per conditions, the modified exposure schedule was associated with higher mean room-temperature strengths, although individual measurements overlapped between exposure conditions. The largest observed difference occurred for vertical specimens at 1100 °C, with retained-strength ratios of 86.1% for the modified schedule and 41.2% for the standard schedule. The combined observations suggest that defect size, morphology, and orientation contribute to the high-temperature response alongside total porosity.

Process-structure-properties of Digital Light Processed Alumina: Effect of Printing Parameters on High Temperature Mechanical Properties / Benelli, A., Tridello, A., Ferraris, M.. - In: CERAMICS INTERNATIONAL. - ISSN 0272-8842. - (2026). [10.1016/j.ceramint.2026.11.299]

Process-structure-properties of Digital Light Processed Alumina: Effect of Printing Parameters on High Temperature Mechanical Properties

Alessandro Benelli;Andrea Tridello;Monica Ferraris
2026

Abstract

Digital light processing (DLP) enables the fabrication of geometrically complex alumina components, but printing-induced defects and build-orientation effects still limit their mechanical reliability, particularly at elevated temperature. This study investigates how exposure parameters and build orientation influence defect evolution, surface topography, elastic stiffness, and flexural strength of DLP-printed alumina. Rectangular bars were manufactured in vertical and horizontal orientations using a standard exposure strategy and the modified condition with a constant exposure energy of 350 mJ cm−2. X-ray computed tomography (XCT) was used to track dimensional changes and XCT-resolved defects after pre-conditioning, debinding, and sintering. Surface topography was evaluated by profilometry, dynamic Young's modulus was measured with Impulse Excitation Technique (IET) from room temperature to 1200 °C, and four-point flexural tests were performed at room temperature and 1100 °C. Exposure modification reduced the sintered XCT-resolved porosity from 0.10 to 0.01% in the vertical orientation and from 0.23 to 0.06% in the horizontal orientation. The median equivalent defect diameter decreased from 85 to 51 μm and from 69 to 42 μm, respectively. Modified specimens exhibited higher dynamic Young's modulus during heating, while all configurations retained approximately 86-88% of their room-temperature stiffness at 1100 °C. Within the limited flexural dataset, based on one or two specimens per conditions, the modified exposure schedule was associated with higher mean room-temperature strengths, although individual measurements overlapped between exposure conditions. The largest observed difference occurred for vertical specimens at 1100 °C, with retained-strength ratios of 86.1% for the modified schedule and 41.2% for the standard schedule. The combined observations suggest that defect size, morphology, and orientation contribute to the high-temperature response alongside total porosity.
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/3018339
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo