This study investigates a comprehensive study on the mechanical and microstructural behavior of cementitious mortars modified with a combination of internal carbonation (via solid CO2), calcined clay as a ceramic pozzolanic additive, and bio-based sheep wool fibers. The investigation aimed to explore sustainable routes for enhancing mortar performance while reducing the environmental impact of cement production. A series of mortars incorporating various combinations of dry ice, calcined clay, and wool fibers was prepared and tested to evaluate compressive and flexural strength, porosity, pore size distribution, phase composition, and microstructural morphology. Results demonstrated that internal carbonation significantly promoted matrix densification and compressive strength, increasing fc by approximately 8% compared to the reference. The addition of calcined clay further improved microstructural compactness, reducing total pore volume by 12%, while the incorporation of wool fibers enhanced post-cracking toughness by over 40% despite a 15–30% decrease in compressive strength. SEM and TGA confirmed the formation of calcite and reduced portlandite content, consistent with carbonation and pozzolanic reactions. The findings underscore the potential and limitations of multicomponent eco-modified cement mortars. Optimizing the balance between internal carbonation, pozzolanic reaction, and fiber stability is a key to developing next-generation low-carbon composites suitable for durable and resilient construction applications

Mechanical and Microstructural Performance of Cement Mortars with Internal Carbonation and Sustainable Additives / Jóźwiak-Niedźwiedzka, D., Lisowski, P., Osial, M., Brachaczek, A., Alterman, D., Fantilli, A.P.. - In: CERAMICS. - ISSN 2571-6131. - 8:4(2025), pp. 1-19. [10.3390/ceramics8040140]

Mechanical and Microstructural Performance of Cement Mortars with Internal Carbonation and Sustainable Additives

Fantilli, Alessandro P.
2025

Abstract

This study investigates a comprehensive study on the mechanical and microstructural behavior of cementitious mortars modified with a combination of internal carbonation (via solid CO2), calcined clay as a ceramic pozzolanic additive, and bio-based sheep wool fibers. The investigation aimed to explore sustainable routes for enhancing mortar performance while reducing the environmental impact of cement production. A series of mortars incorporating various combinations of dry ice, calcined clay, and wool fibers was prepared and tested to evaluate compressive and flexural strength, porosity, pore size distribution, phase composition, and microstructural morphology. Results demonstrated that internal carbonation significantly promoted matrix densification and compressive strength, increasing fc by approximately 8% compared to the reference. The addition of calcined clay further improved microstructural compactness, reducing total pore volume by 12%, while the incorporation of wool fibers enhanced post-cracking toughness by over 40% despite a 15–30% decrease in compressive strength. SEM and TGA confirmed the formation of calcite and reduced portlandite content, consistent with carbonation and pozzolanic reactions. The findings underscore the potential and limitations of multicomponent eco-modified cement mortars. Optimizing the balance between internal carbonation, pozzolanic reaction, and fiber stability is a key to developing next-generation low-carbon composites suitable for durable and resilient construction applications
2025
File in questo prodotto:
File Dimensione Formato  
ceramics-08-00140-v2.pdf

accesso aperto

Tipologia: 2a Post-print versione editoriale / Version of Record
Licenza: Creative commons
Dimensione 2.87 MB
Formato Adobe PDF
2.87 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/3013517