Slow pyrolysis is a promising technology to convert sewage sludge into char: a stable solid product with high carbon and phosphorus content. However, due to its heavy metals content, char use in agriculture is avoided in many European Union (EU) countries. This study aimed to test a solution, based on integrating slow pyrolysis and chemical leaching, to separate phosphorus and other inorganics from char, obtaining an inorganic P-rich fertiliser and a C-rich solid usable for industrial purposes. The sludge was first characterized and then processed in a 3 kg/h slow pyrolysis reactor at 450 °C for 30 min. The resulting char was processed by chemical leaching with acid (HCl, HNO3) and alkali (KOH) reagents to extract inorganic compounds. To optimize the inorganic extraction, three case studies have been considered. The char obtained from sewage sludge pyrolysis contained around 78% d.b. (dry basis) of inorganics, 14% d.b. of C, 14% d.b. of Al, and almost 5% d.b. of P. The leaching tests enabled to extract 100% of P, Mg, and Ca from the char. The remaining char contained mainly carbon (27%) and silica (42%), with a surface area of up to 70 m2/g, usable as adsorbent or precursor of sustainable materials.
Opportunities of Integrating Slow Pyrolysis and Chemical Leaching for Extraction of Critical Raw Materials from Sewage Sludge / Salimbeni, A.; Di Bianca, M.; Lombardi, G.; Rizzo, A. M.; Chiaramonti, D.. - In: WATER. - ISSN 2073-4441. - 15:6(2023). [10.3390/w15061060]
Opportunities of Integrating Slow Pyrolysis and Chemical Leaching for Extraction of Critical Raw Materials from Sewage Sludge
Rizzo A. M.;Chiaramonti D.
2023
Abstract
Slow pyrolysis is a promising technology to convert sewage sludge into char: a stable solid product with high carbon and phosphorus content. However, due to its heavy metals content, char use in agriculture is avoided in many European Union (EU) countries. This study aimed to test a solution, based on integrating slow pyrolysis and chemical leaching, to separate phosphorus and other inorganics from char, obtaining an inorganic P-rich fertiliser and a C-rich solid usable for industrial purposes. The sludge was first characterized and then processed in a 3 kg/h slow pyrolysis reactor at 450 °C for 30 min. The resulting char was processed by chemical leaching with acid (HCl, HNO3) and alkali (KOH) reagents to extract inorganic compounds. To optimize the inorganic extraction, three case studies have been considered. The char obtained from sewage sludge pyrolysis contained around 78% d.b. (dry basis) of inorganics, 14% d.b. of C, 14% d.b. of Al, and almost 5% d.b. of P. The leaching tests enabled to extract 100% of P, Mg, and Ca from the char. The remaining char contained mainly carbon (27%) and silica (42%), with a surface area of up to 70 m2/g, usable as adsorbent or precursor of sustainable materials.File | Dimensione | Formato | |
---|---|---|---|
water-15-01060.pdf
accesso aperto
Tipologia:
2a Post-print versione editoriale / Version of Record
Licenza:
Creative commons
Dimensione
1.21 MB
Formato
Adobe PDF
|
1.21 MB | Adobe PDF | Visualizza/Apri |
Pubblicazioni consigliate
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.
https://hdl.handle.net/11583/2995496