A set of quartz crystal microbalances (QMB) was used at JET with full carbon wall to monitor mass erosion/ deposition rates in the remote areas of the divertor. After introduction of the ITER-like wall (ILW) in JET with beryllium main wall and tungsten divertor, strong reduction of the material deposition and accompanied fuel retention was observed. Therefore the existing QMB electronics have been modified to improve the accuracy of frequency measurements by a factor of ten down to 0.1 Hz which corresponds to 1.4 ng cm(-2). The averaged deposition rates of 1.2-3 ng cm(-2) s(-1) and erosion rates of 5.6-8.1 ng cm(-2) s(-1) were observed in the inner divertor of JET-ILW with the inner strike point positions close to the bottom edge of vertical tile 3 and at the horizontal tile 4 respectively. The erosion with averaged rates of approximate to 2.1 ng cm(-2) s(-1) and approximate to 120 ng cm(-2) s(-1) were observed in the outer divertor for the outer strike point positions at tile 5 and tile 6 respectively. (C) 2017 The Authors. Published by Elsevier Ltd. This is an open access article under the CC BY-NC-ND license.

Quartz micro-balance results of pulse-resolved erosion/deposition in the JET-ILW divertor / Sergienko, G.; Esser, H. G.; Kirschner, A.; Huber, A.; Freisinger, M.; Brezinsek, S.; Widdowson, A.; Ayres, Ch.; Weckmann, A.; Heinola, K.; Subba, F.. - In: NUCLEAR MATERIALS AND ENERGY. - ISSN 2352-1791. - 12:(2017), pp. 478-482. [10.1016/j.nme.2017.03.007]

Quartz micro-balance results of pulse-resolved erosion/deposition in the JET-ILW divertor

Subba, F.
2017

Abstract

A set of quartz crystal microbalances (QMB) was used at JET with full carbon wall to monitor mass erosion/ deposition rates in the remote areas of the divertor. After introduction of the ITER-like wall (ILW) in JET with beryllium main wall and tungsten divertor, strong reduction of the material deposition and accompanied fuel retention was observed. Therefore the existing QMB electronics have been modified to improve the accuracy of frequency measurements by a factor of ten down to 0.1 Hz which corresponds to 1.4 ng cm(-2). The averaged deposition rates of 1.2-3 ng cm(-2) s(-1) and erosion rates of 5.6-8.1 ng cm(-2) s(-1) were observed in the inner divertor of JET-ILW with the inner strike point positions close to the bottom edge of vertical tile 3 and at the horizontal tile 4 respectively. The erosion with averaged rates of approximate to 2.1 ng cm(-2) s(-1) and approximate to 120 ng cm(-2) s(-1) were observed in the outer divertor for the outer strike point positions at tile 5 and tile 6 respectively. (C) 2017 The Authors. Published by Elsevier Ltd. This is an open access article under the CC BY-NC-ND license.
File in questo prodotto:
File Dimensione Formato  
1-s2.0-S2352179116301181-main.pdf

accesso aperto

Tipologia: 2a Post-print versione editoriale / Version of Record
Licenza: Creative commons
Dimensione 1.1 MB
Formato Adobe PDF
1.1 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/2986916