The effect of building orientation on the very-high-cycle fatigue (VHCF) response of Ti-6Al-4V specimens produced through selective laser melting (SLM) process with three different building orientations (0°, 45° and 90°) has been experimentally assessed. The fatigue performance decreases with different building orientations from 0° to 90°. The fatigue crack origin has been found to be always an internal defect both at high-cycle fatigue and VHCF regime independent of building orientations. Size of defects induced fatigue failures and the stress intensity factor range decrease with the number of cycles to failure. By considering the VHCF strength at 109 cycles, the median value decreases from 217 MPa (0°) to 201 MPa (45°) and finally to 155 MPa (90°), with a 40% reduction from 0° to 90°. The building orientation significantly influences both the defect size and the resulting VHCF response.

Very-high-cycle fatigue behavior of Ti-6Al-4V manufactured by selective laser melting: Effect of build orientation / Qian, G.; Li, Y.; Paolino, D. S.; Tridello, A.; Berto, F.; Hong, Y.. - In: INTERNATIONAL JOURNAL OF FATIGUE. - ISSN 0142-1123. - STAMPA. - 136:105628(2020). [10.1016/j.ijfatigue.2020.105628]

Very-high-cycle fatigue behavior of Ti-6Al-4V manufactured by selective laser melting: Effect of build orientation

Paolino D. S.;Tridello A.;
2020

Abstract

The effect of building orientation on the very-high-cycle fatigue (VHCF) response of Ti-6Al-4V specimens produced through selective laser melting (SLM) process with three different building orientations (0°, 45° and 90°) has been experimentally assessed. The fatigue performance decreases with different building orientations from 0° to 90°. The fatigue crack origin has been found to be always an internal defect both at high-cycle fatigue and VHCF regime independent of building orientations. Size of defects induced fatigue failures and the stress intensity factor range decrease with the number of cycles to failure. By considering the VHCF strength at 109 cycles, the median value decreases from 217 MPa (0°) to 201 MPa (45°) and finally to 155 MPa (90°), with a 40% reduction from 0° to 90°. The building orientation significantly influences both the defect size and the resulting VHCF response.
File in questo prodotto:
File Dimensione Formato  
IJF_2020.pdf

non disponibili

Tipologia: 2a Post-print versione editoriale / Version of Record
Licenza: Non Pubblico - Accesso privato/ristretto
Dimensione 6.44 MB
Formato Adobe PDF
6.44 MB Adobe PDF   Visualizza/Apri   Richiedi una copia
IJF_2020_Qian_embargo.pdf

Open Access dal 29/03/2022

Descrizione: Post-print Embargo
Tipologia: 2. Post-print / Author's Accepted Manuscript
Licenza: Creative commons
Dimensione 2.72 MB
Formato Adobe PDF
2.72 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/2813246