In this work, three new glass-ceramic compositions are designed and characterized as sealant materials for solid oxide electrolysis cells (SOEC), having operating temperature of 850°C. The crystallization and the sintering behavior of the glasses are investigated by using differential thermal analysis (DTA) and heating stage microscopy (HSM) respectively. The glasses show glass transition temperatures of 715-740°C, while the coefficients of thermal expansion (CTE) of 9.3-10.3 x 10-6 K-1 (200-500°C) are measured for the glass-ceramics, matching with the CTEs of the other cell components. The compatibility between the glassceramic sealants, the 3YSZ electrolyte and the Crofer22APU interconnect is examined by means of SEM and EDS, in the as-joined condition and after 1000 hours at 850°C in air. Compositional changes in the glass-ceramic sealants are reviewed and discussed with respect to the formed crystalline phases before and after the aging treatment at 850°C.

Design and characterization of novel glass-ceramic sealants for solid oxide electrolysis cell (SOEC) applications / Javed, Hassan; Sabato, Antonio Gianfranco; Herbrig, Kai; Ferrero, Domenico; Walter, Christian; Salvo, Milena; Smeacetto, Federico. - In: INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY. - ISSN 1546-542X. - 15:4(2018), pp. 999-1010. [10.1111/ijac.12889]

Design and characterization of novel glass-ceramic sealants for solid oxide electrolysis cell (SOEC) applications

Javed, Hassan;Sabato, Antonio Gianfranco;Ferrero, Domenico;Salvo, Milena;Smeacetto, Federico
2018

Abstract

In this work, three new glass-ceramic compositions are designed and characterized as sealant materials for solid oxide electrolysis cells (SOEC), having operating temperature of 850°C. The crystallization and the sintering behavior of the glasses are investigated by using differential thermal analysis (DTA) and heating stage microscopy (HSM) respectively. The glasses show glass transition temperatures of 715-740°C, while the coefficients of thermal expansion (CTE) of 9.3-10.3 x 10-6 K-1 (200-500°C) are measured for the glass-ceramics, matching with the CTEs of the other cell components. The compatibility between the glassceramic sealants, the 3YSZ electrolyte and the Crofer22APU interconnect is examined by means of SEM and EDS, in the as-joined condition and after 1000 hours at 850°C in air. Compositional changes in the glass-ceramic sealants are reviewed and discussed with respect to the formed crystalline phases before and after the aging treatment at 850°C.
File in questo prodotto:
File Dimensione Formato  
Javed_et_al-2018-International_Journal_of_Applied_Ceramic_Technology.pdf

accesso aperto

Descrizione: articolo principale
Tipologia: 2a Post-print versione editoriale / Version of Record
Licenza: Creative commons
Dimensione 2.43 MB
Formato Adobe PDF
2.43 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/2705355
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo