Two pressureless and reliable procedures for brazing SiC-based materials have been designed. The joining was obtained by the in-situ formation of a Ti3Si(Al)C2 MAX phase using simple Al-Ti interlayers. Wettability studies were conducted using several Al-Ti alloys in contact with SiC at 1500 °C. The interfacial microstructures and thermodynamic analysis demonstrated that liquid Al3Ti in contact with SiC formed a well-bonded Ti3Si(Al)C2 interfacial layer. These findings guided the design of two joining methods: one consisted of the simple infiltration of Al3Ti into the brazing seam, while an Al3Ti paste/Ti/Al3Ti paste interlayer assembly was designed for the second process. Sound interfaces without cracks were obtained in both processes. The average shear strength was very high, 296 MPa, for the infiltration method; the drawback was the presence of residual Al. Joining through Al3Ti/Ti/Al3Ti interlayers avoided the presence of low-temperature melting phases, with lower shear strength: 85 or 89 MPa depending on the testing method.

Wetting of SiC by Al-Ti alloys and joining by in-situ formation of interfacial Ti3Si(Al)C2 / Valenza, Fabrizio; Gambaro, Sofia; Muolo, Maria Luigia; Salvo, Milena; Casalegno, Valentina. - In: JOURNAL OF THE EUROPEAN CERAMIC SOCIETY. - ISSN 0955-2219. - 38:11(2018), pp. 3727-3734. [10.1016/j.jeurceramsoc.2018.04.025]

Wetting of SiC by Al-Ti alloys and joining by in-situ formation of interfacial Ti3Si(Al)C2

Salvo, Milena;Casalegno, Valentina
2018

Abstract

Two pressureless and reliable procedures for brazing SiC-based materials have been designed. The joining was obtained by the in-situ formation of a Ti3Si(Al)C2 MAX phase using simple Al-Ti interlayers. Wettability studies were conducted using several Al-Ti alloys in contact with SiC at 1500 °C. The interfacial microstructures and thermodynamic analysis demonstrated that liquid Al3Ti in contact with SiC formed a well-bonded Ti3Si(Al)C2 interfacial layer. These findings guided the design of two joining methods: one consisted of the simple infiltration of Al3Ti into the brazing seam, while an Al3Ti paste/Ti/Al3Ti paste interlayer assembly was designed for the second process. Sound interfaces without cracks were obtained in both processes. The average shear strength was very high, 296 MPa, for the infiltration method; the drawback was the presence of residual Al. Joining through Al3Ti/Ti/Al3Ti interlayers avoided the presence of low-temperature melting phases, with lower shear strength: 85 or 89 MPa depending on the testing method.
File in questo prodotto:
File Dimensione Formato  
1-s2.0-S0955221918302371-main.pdf

non disponibili

Tipologia: 2a Post-print versione editoriale / Version of Record
Licenza: Non Pubblico - Accesso privato/ristretto
Dimensione 6.8 MB
Formato Adobe PDF
6.8 MB Adobe PDF   Visualizza/Apri   Richiedi una copia
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/2706801
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo